Works perfect for me :) Thanks



Just needed to replace the broken left one.
Probably should have printed on a smooth plate, but what's done is done. Works well!
Works and looks great.
0.4mm nozzle
Inland Glass Orange PLA
15% infill gyroid
Printed in PLA with a .4mm nozzle at .1mm layer height. Mechanism works great.
Might add color accents later since I now know that it works great as a replacement. (edited)
I printed the right piece in PLA using a 0.12 mm layer height, and using a really slow speed (5 mm/s) for the first layer in order to ensure that the details could be replicated. I was printed really fina with a 0.4 mm nozzle and the result is really appealing.
I hope PLA will make the job done, otherwise I will print it in ABS/ASA.
Thanks!
@Botvinnik Mine are PLA and are still running strong since July last year. Thank you for the 5 stars!
Nice print, thanks for sharing! I think it came out with great detail even with the default 0.4mm nozzle.